ʻO CCS25 FeCuSn ka pauda i hoʻopili mua ʻia no ka lāʻau marble kiʻekiʻe

wehewehe pōkole:

He aha ka CCS25 pre-alloyed metala pauka?ʻO CCS25 ʻo Cu, Co, Sn i hoʻohui ʻia i ka pauka mua i hoʻohui ʻia, nona kahi ʻano hoʻoheheʻe maikaʻi, unifor a me ka hoʻopaʻa paʻa ʻana i ke daimana, suitale no ka hana ʻana i ka ʻoki ʻoki marble kiʻekiʻe.2. Nā palena o CSS25 pauka Main Element Cu, Co, Sn Theoretical Density 8.29g/cm³ Sintering Temperature 760 ℃ Ka ikaika moe 800 MPa Hardness 85-95HRB 3. Applicaiton Instuctions —Maring a marble sa...


Huahana Huahana

Huahana Huahana

  1. He aha ka CCS25 pre-alloyed metala pauka?

ʻO CCS25 ka Cu, Co, Sn i hui ʻiaka pauka i hui mua ia, nona ka maikai, unifor a me ka compact sintering hale, he nui ka pulupulu a me ka paa ana i ka daimana, suitale no ka hana ana i ke kiʻekiʻe kiʻekiʻe marble oki maka.

2. Nā palena o ka pauka CSS25

Mea Nui Cu, Co, Sn
ʻO ka Density Theoretical 8.29g/cm³
Ka Mahana Sintering 760 ℃
Ka ikaika moe 800 MPa
ʻoʻoleʻa 85-95HRB

3. Nā ʻōlelo aʻoaʻo noiʻi —Ka hōʻailona ʻana i kahi pahi ʻili kinikini

A. Paneka Metala Pauda

CCS25—-50-70%

Cu——–25-35%

Sn——–4-7%

    

B. Daimana

50/60—-30%

60/70—-40%

70-80—-30%

C. 'ē aʻe

ʻO ka manaʻo daimana: 20-25%

Ka Mahana Sintering: 760-780 ℃